selected scholarly activity
-
books
-
chapters
- Corrosion. 139-218. 2018
- Environmentally assisted cracking. 219-256. 2018
- Experimental methodologies. 19-43. 2018
- Introduction. 1-17. 2018
- Radiation effects and mechanical properties. 45-78. 2018
- Water chemistry. 79-138. 2018
- Effect of Cold Work on the Corrosion Resistance of an Austenitic Stainless Steel. 127-133. 2016
- Subsurface De‐alloying during SCW Exposure. 103-112. 2014
- Effect of some Microstructural Parameters on the Corrosion Resistance of Magnesium Alloys. 271-276. 2012
- 19 Stress corrosion cracking in pipelines. 749-771. 2011
- Contributor contact details. xiii-xvii. 2011
- Stress corrosion cracking in pipelines. 749-771. 2011
-
conferences
- Ageing-related pipeline failures and safety assurance technologies. Conference Proceedings of the 8th International Symposium on Project Management Ispm 2020. 614-622. 2020
- Lateral Confinement Effects on the Axial Compressive Strength of Mortar Specimen. Procedia Engineering. 2470-2475. 2017
- Full-Scale Stress Corrosion Crack Growth Testing of an X70 Spiral-Welded Pipe in Near-Neutral pH Soil Environment. Volume 1: Pipelines and Facilities Integrity. V001T03A022-V001T03A022. 2016
- EFFECT OF COLD WORK ON THE CORROSION RESISTANCE OF AN AUSTENITIC STAINLESS STEEL. TMS Annual Meeting. 127-133. 2016
- Advances in materials evaluation for the Canadian SCWR core concept. 36th Annual CNS Conference and 40th CNS Cna Student Conference Nuclear in the 21st Century Global Directions and Canada S Role. 2016
- Assessment of Candidate Fuel Cladding Alloys for the Canadian Supercritical Water-Cooled Reactor Concept. Journal of Nuclear Engineering and Radiation Science. 2016
- Constructing a Grain Boundary Sensitization-Embrittlement Map for Type 310S Stainless Steel Fuel Cladding in the Canadian SCWR Concept. 36th Annual CNS Conference and 40th CNS Cna Student Conference Nuclear in the 21st Century Global Directions and Canada S Role. 2016
- Development of a CanmetMATERIALS Gen IV Materials Property Database for Materials Selection. 36th Annual CNS Conference and 40th CNS Cna Student Conference Nuclear in the 21st Century Global Directions and Canada S Role. 2016
- A Simulation Study about the Effects of Temperature on Compression Stress Relaxation for Natural Rubber (NR). MACHINERY, MATERIALS SCIENCE AND ENERGY ENGINEERING. 492-498. 2015
- Corrosion and stress corrosion cracking of UNS S31008 and UNS N08810 alloys in supercritical water. NACE - International Corrosion Conference Series. 1-15. 2015
- Corrosion assessment of high temperature alloys for SCWR fuel cladding design. Materials Science and Technology Conference and Exhibition 2015 MS and T 2015. 1233-1240. 2015
- TEM Study of Supercritical Water Corrosion in 310S and 800H Alloys. Microscopy and Microanalysis. 1866-1867. 2014
- Subsurface De‐alloying during SCW Exposure. CHARACTERIZATION OF MINERALS, METALS, AND MATERIALS 2014. 103-112. 2014
- SCW Corrosion Resistance of Candidate Stainless Steels. TMS Annual Meeting. 319-326. 2013
- Effects of grain size and CeO2 addition on the corrosion behaviour of Cr2O3 based ceramics in high temperature supercritical water environment. Canadian Nuclear Society 33rd Annual Conference of the Canadian Nuclear Society and 36th CNS Cna Student Conference 2012 Building on Our Past Building for the Future. 1576-1580. 2012
- Oxidation and stress corrosion cracking initiation of austenitic alloys in supercritical water. Canadian Nuclear Society 33rd Annual Conference of the Canadian Nuclear Society and 36th CNS Cna Student Conference 2012 Building on Our Past Building for the Future. 1606-1611. 2012
- The influences of ultrasonic peening treatment on oxidation of designed F/M steels in supercritical water. Canadian Nuclear Society 33rd Annual Conference of the Canadian Nuclear Society and 36th CNS Cna Student Conference 2012 Building on Our Past Building for the Future. 1408-1413. 2012
- Effects of surface modifications on SCW corrosion resistance. TMS Annual Meeting. 43-48. 2012
- Effect of some Microstructural Parameters on the Corrosion Resistance of Magnesium Alloys. Magnesium Technology. 271-276. 2012
- Effects of Surface Modifications on SCW Corrosion Resistance. CHARACTERIZATION OF MINERALS, METALS, AND MATERIALS. 43-48. 2012
- Effect of coating and surface modification on the corrosion resistance of selected alloys in supercritical water. Canadian Nuclear Society 32nd Annual Conference of the Canadian Nuclear Society and 35th CNS can Student Conference 2011. 872-878. 2011
- Filling the gaps in SCWR materials research: Advanced nuclear corrosion research facilities in Hamilton. Canadian Nuclear Society 32nd Annual Conference of the Canadian Nuclear Society and 35th CNS can Student Conference 2011. 837-846. 2011
- Effect of Cr Content on Corrosion Resistance of Experimental Fe‐Cr Alloys under SCW Condition. EPD CONGRESS 2011. 143-148. 2011
- A CONCRETE TENSION FAILURE MODEL UNDER IMPACT LOADING. BALLISTICS 2011: 26TH INTERNATIONAL SYMPOSIUM ON BALLISTICS, VOL 1 AND VOL 2. 1617-1624. 2011
- Characterization of thin passive film formed on inconel-625 tested in SCW. TMS Annual Meeting. 51-58. 2010
- Research and development initiatives in support of the conceptual design for the CANDU supercritical water-cooled reactor. Canadian Nuclear Society 31st Annual Conference of the Canadian Nuclear Society and 34th CNS Cna Student Conference 2010. 1216-1229. 2010
- Materials Research in Support of SCWR Development: Current Areas, Gaps and Needs. 18th International Conference on Nuclear Engineering: Volume 6. 233-+. 2010
- Canada's NSERC/NRCan/AECL generation IV energy technologies program. Canadian Nuclear Society 30th Annual Canadian Nuclear Society Conference and 33rd CNS Cna Student Conference 2009. 1350-1362. 2009
- Stress corrosion cracking of oil and gas pipelines: New insights on crack growth behaviour gained from full-scale and small scale tests. 12th International Conference on Fracture 2009 Icf 12. 3340-3347. 2009
- The influence of weld heat-affected zone on stress corrosion cracking of pipeline steel in near-neutral pH environment. NACE - International Corrosion Conference Series. 085001-0850011. 2008
- Effects of surface contamination and pre-exposure on the corrosion rate of Mg alloys. TMS Annual Meeting. 31-38. 2007
- Electrochemical study of magnesium hydride formation in aqueous solution. TMS Annual Meeting. 21-30. 2007
- Intelligent pipeline monitoring system. NACE - International Corrosion Conference Series. 072671-0726711. 2007
- Corrosion Protection of Joining Areas in Magnesium Die-Cast and Sheet Products. Materials Science Forum. 523-528. 2007
- Theoretical research on Ni-like Ag 13.9nm X-ray laser driven by 3 mu m and 6 mu m wavelength laser. Springer proceedings in physics. 295-+. 2007
- Theoretical research on enhancement of gain for Ni-like Ag 13.9nm X-Ray laser using a new two-layer target. Springer proceedings in physics. 311-+. 2007
- Corrosion Fatigue of AM50 and AE44 Alloys at Various Temperature and R-Ratio. SAE Technical Papers. 2006
- Near-Neutral pH SCC of Two Line Pipe Steels Under Quasi-Static Stressing Conditions. Volume 2: Integrity Management; Poster Session; Student Paper Competition. 95-105. 2006
- Performance of Candidate Materials and Coatings for Thermal Management Systems for Proton Exchange Membrane Fuel Cells. SAE Technical Papers. 2006
- Corrosion Protection of Structural Magnesium Alloys: Recent Development. SAE Technical Papers. 2005
- Protection of Mg Alloys against Galvanic and Other Forms of Corrosion. Materials Science Forum. 787-792. 2005
- A robust approach to discard feature outliers using M-estimator method. PROCEEDINGS OF THE THIRD INTERNATIONAL SYMPOSIUM ON INSTRUMENTATION SCIENCE AND TECHNOLOGY, VOL 2. 265-268. 2004
- Experimental Study on SCC Susceptibility of X60 Steel Using Full Pipe Sections in Near-Neutral pH Environment. 2004 International Pipeline Conference, Volumes 1, 2, and 3. 133-141. 2004
- Protection of Mg Alloys for Structural Applications in Automobiles. SAE Technical Papers. 2004
- The research of the biomaterials' rapid forming machines. ICMA 2002 INTERNATIONAL CONFERENCE ON MANUFACTURING AUTOMATION. 419-424. 2002
- Magnetic properties of SmCo/Cr thin films with Cr under different preparation conditions. Materials Science & Engineering: A. 1043-1045. 2001
- Magnetic properties of SmCo/Fe/SmCo trilayer films. Materials Science & Engineering: A. 969-971. 2001
- Stress Corrosion Cracking of Linepipe Steels in Near-Neutral pH Environment: A Review of the Effects of Stress. ASTM Special Technical Publication. 473-483. 2000
- The roles of stress in SCC of linepipe steels in near-neutral pH environment. ENVIRONMENTALLY INDUCED CRACKING OF METALS, PROCEEDINGS. 93-102. 2000
- Environment-assisted cracking of oil and gas pipelines - A review. FATIGUE '99: PROCEEDINGS OF THE SEVENTH INTERNATIONAL FATIGUE CONGRESS, VOLS 1-4. 2285-2291. 1999
- Influence of FeCo-interlayer thickness on remanence and coercivity in SmCo/FeCo/SmCo triple-layer films. IEEE Transactions on Magnetics. 3331-3333. 1999
- Effects of Hydrostatic Testing on the Growth of Stress-Corrosion Cracks. Volume 1: Risk Assessment and Management; Emerging Issues and Innovative Projects; Operations and Maintenance; Corrosion and Integrity Management. 459-472. 1998
- Effects of pressure fluctuation on the growth of stress corrosion cracks in an X-52 linepipe steel. Proceedings of the International Conference on Pressure Vessel Technology ICPVT. 321-326. 1996
- Pipeline SCC in Near-Neutral pH Environment: Recent Progress. Volume 1: Regulations, Codes, and Standards; Current Issues; Materials; Corrosion and Integrity. 485-493. 1996
- Pipeline SCC in near-neutral pH environment: Results of full-scale tests. NACE - International Corrosion Conference Series. 1996
- Methodology for realistic full-scale testing of linepipe for stress-corrosion cracking. PIPELINE TECHNOLOGY, VOLS I AND II. A571-A576. 1995
- The Stress Corrosion Cracking of Annealed Type 316 Stainless Steel in High Temperature Water. 1-12. 1990
-
journal articles
- Design of high temperature oxidation-resistant high-entropy alloys via machine learning and natural mixing process. Corrosion Science. 255:113047. 2025
- Degradation behavior of a 12 % Cr tempered martensite ferritic steel after 20 years of service. International Journal of Pressure Vessels and Piping. 214:105437. 2025
- A comparative study of hydrogen embrittlement susceptibility of X60 pipeline base metal and its weld joints made by rotary friction welding. Journal of Materials Research and Technology. 35:6728-6738. 2025
- The formation of strain-induced martensite and its influence on hydrogen compatibility of metastable austenitic stainless steels: A state-of knowledge review. Journal of Science: Advanced Materials and Devices. 10:100842. 2025
- Assessing the effects of loading rate on fracture toughness of AISI 1020 and API 5L X80 steels with hydrogen charging: experimental and numeric simulation study. Engineering Fracture Mechanics. 314:110771. 2025
- Insights into the precipitation-dominated creep behavior of a 25Cr20Ni-Nb-N austenitic heat-resistant steel via interrupted creep. Materials Science & Engineering: A. 919:147520. 2025
- Direct observation of the evolution behavior of micro to nanoscale precipitates in austenitic heat-resistant steel via electron channeling contrast imaging. Materials Characterization. 218:114550. 2024
- Effect of heat input on the microstructure and hydrogen embrittlement susceptibility of the coarse-grain heat-affected zone of CrMo steels generated using a Gleeble 3500 welding simulator. Engineering Failure Analysis. 166:108868. 2024
- Stress-Corrosion-Cracking Sensitivity of the Sub-Zones in X80 Steel Welded Joints at Different Potentials. Materials. 17:3481-3481. 2024
- The migration of jet materials along the collision interface with laser impact welding. Journal of Manufacturing Processes. 122:1-6. 2024
- Change in Hydrogen Trapping Characteristics and Influence on Hydrogen Embrittlement Sensitivity in a Medium-Carbon, High-Strength Steel: The Effects of Heat Treatments.. Materials. 17:1854. 2024
- Improved Bending Strength and Thermal Conductivity of Diamond/Al Composites with Ti Coating Fabricated by Liquid–Solid Separation Method. Materials. 17:1485-1485. 2024
- Data Augmentation of a Corrosion Dataset for Defect Growth Prediction of Pipelines Using Conditional Tabular Generative Adversarial Networks. Materials. 17:1142-1142. 2024
- The role of α′-martensite on the variation of compressive residual stress in a gradient nanostructured austenitic stainless steel. Materials and Design. 238:112723-112723. 2024
- Effects of tempering temperature on the precipitation behaviors of nanoparticles and their influences on the susceptibility to hydrogen embrittlement of a Cr–Mo–V steel. International Journal of Hydrogen Energy. 50:254-269. 2024
- Investigating the thermal stability of compressive residual stress in a gradient nanostructured austenitic stainless steel by in-situ XRD and TEM. Materials Characterization. 207:113610-113610. 2024
- Electrochemical potential dependence of SCC initiation in X60 pipeline steel in near-neutral pH environment. Journal of Materials Research and Technology. 27:4950-4961. 2023
- The effect of surface grinding and Si addition on the corrosion of Fe-12Cr ODS steels in supercritical CO2. Corrosion Science. 224:111533-111533. 2023
- Externally-Physical-Field-Assisted Aging Precipitation in Aerospace Aluminum Alloys: A Review. Critical Reviews in Solid State and Materials Sciences. 48:535-560. 2023
- Effect of laser shock peening and surface mechanical attrition treatment on the oxidation resistance of a 20Cr-25Ni-Nb stainless steel. Materials Characterization. 203:113065-113065. 2023
- A new hybrid approach model for predicting burst pressure of corroded pipelines of gas and oil. Engineering Failure Analysis. 149:107248-107248. 2023
- The achievement of lap weld and gap control for laser impact welding with water as the confinement layer. Journal of Manufacturing Processes. 95:105-114. 2023
- Advances in corrosion growth modeling for oil and gas pipelines: A review. Process Safety and Environmental Protection: Transactions of the Institution of Chemical Engineers, Part B. 171:71-86. 2023
- Variety of microstructure and mechanical properties along the laser impact welded interface. Science and Technology of Welding and Joining. 28:128-136. 2023
- Understanding the excellent corrosion resistance of Fe-12Cr ODS alloys with and without Si in supercritical CO2 through advanced characterization. Corrosion Science. 210:110827-110827. 2023
- Research and demonstration on hydrogen compatibility of pipelines: a review of current status and challenges. International Journal of Hydrogen Energy. 47:28585-28604. 2022
- Microstructural Effects in the Development of Near-Neutral pH Stress Corrosion Cracks in Pipelines. Materials. 15:4372-4372. 2022
- Microstructure complexities of laser impact welded Al-Ti bonding interface. Scripta Materialia. 211:114488-114488. 2022
- Effects of Heat Treatment on the Microstructure and Mechanical Properties of a Novel H-Grade Sucker Rod Steel. Metals. 12:294-294. 2022
- Effect of applied low-voltage spatial electric field on the corrosion behaviour of copper in 3.5 wt-% NaCl solution. Corrosion Engineering Science and Technology. 57:74-84. 2022
- Improvement of thermal conductivity of diamond/Al composites by optimization of liquid-solid separation process. Journal of Materials Processing Technology. 297:117267-117267. 2021
- Effect of Diamond Particle Size on the Thermal Properties of Diamond/Al Composites for Packaging Substrate. Jinshu Xuebao/Acta Metallurgica Sinica. 57:937-947. 2021
- Fabrication of Functionally Graded Diamond/Al Composites by Liquid–Solid Separation Technology. Materials. 14:3205-3205. 2021
- Effect of surface mechanical attrition treatment on stainless steel corrosion. Surface Engineering. 37:739-748. 2021
- Effect of heat treatment process on microstructure and properties of KD sucker rod steel. Jinshu Rechuli/Heat Treatment of Metals. 46:28-31. 2021
- Creep behavior of an alumina-forming austenitic steel with simple alloy design. Materials Today Communications. 25:101303-101303. 2020
- Progress in dispersoids distribution precipitating during homogenising Zr-containing Al–Cu–Li and Al–Zn–Mg alloys. Materials Science and Technology. 36:1903-1921. 2020
- Research Status and Prospect of Laser Impact Welding. Metals. 10:1444-1444. 2020
- Microstructure and mechanical behaviors of grinding balls produced by dual matrix structure two-step austempering process. Journal of Materials Research and Technology. 9:4672-4681. 2020
- Effects of Si, Mn on the corrosion behavior of ferritic–martensitic steels in supercritical water (SCW) environments. Corrosion Science. 166:108432-108432. 2020
- Mechanical properties evaluation and plastic instabilities of Fe-9%Cr ODS steels. Fusion Engineering and Design. 149:111335-111335. 2019
- Fabrication of superhydrophobic surfaces for corrosion protection: A review. Materials Science and Technology. 35:313-326. 2019
- Stress corrosion cracking susceptibility of thermally-aged Type 310S stainless steels in supercritical water. Corrosion Science. 135:1-11. 2018
- Effect of Thermal Aging on the Intergranular Stress Corrosion Cracking Susceptibility of Type 310S Stainless Steel. Corrosion. 74:430-443. 2018
- The in-depth residual strain heterogeneities due to an indentation and a laser shock peening for Ti-6Al-4V titanium alloy. Materials Science & Engineering: A. 714:140-145. 2018
- Characterization of oxide layer and micro-crack initiation in alloy 316L stainless steel after 20,000 h exposure to supercritical water at 500 °C. Materials Characterization. 131:532-543. 2017
- Corrosion behavior of alloy 316L stainless steel after exposure to supercritical water at 500 °C for 20,000 h. Journal of Supercritical Fluids. 127:191-199. 2017
- Internal oxidation and crack susceptibility of alloy 310S stainless steel after long term exposure to supercritical water at 500°C. Journal of Supercritical Fluids. 120:161-172. 2017
- A comparative study on the oxidation of austenitic alloys 304 and 304-oxide dispersion strengthened steel in supercritical water at 650 °C. Journal of Supercritical Fluids. 119:245-260. 2017
- A REVIEW OF IRRADIATION EFFECTS ON MECHANICAL PROPERTIES OF CANDIDATE SCWR FUEL CLADDING ALLOYS FOR DESIGN CONSIDERATIONS. CNL NUCLEAR REVIEW. 5:309-331. 2016
- Characterization of oxide scales grown on alloy 310S stainless steel after long term exposure to supercritical water at 500 °C. Materials Characterization. 120:273-284. 2016
- Stability of Chromia (Cr2O3)-Based Scales Formed During Corrosion of Austenitic Fe-Cr-Ni Alloys in Flowing Oxygenated Supercritical Water. Corrosion. 72:1170-1180. 2016
- Erratum to: Initiation of Stress Corrosion Cracks in X80 and X100 Pipe Steels in Near-Neutral pH Environment. Journal of Materials Engineering and Performance. 25:3546-3547. 2016
- A comparative study of oxide scales grown on stainless steel and nickel-based superalloys in ultra-high temperature supercritical water at 800 °C. Corrosion Science. 106:188-207. 2016
- The reproducibility of corrosion testing in supercritical water—Results of an international interlaboratory comparison exercise. Corrosion Science. 106:147-156. 2016
- Materials Assessment for the Canadian SCWR Core Concept. JOM. 68:456-462. 2016
- Microstructure Instability of Candidate Fuel Cladding Alloys: Corrosion and Stress Corrosion Cracking Implications. JOM. 68:485-489. 2016
- Effect of Thermal Pretreatment on the Corrosion of Stainless Steel in Flowing Supercritical Water. Journal of Nuclear Engineering and Radiation Science. 2. 2016
- Initiation of Stress Corrosion Cracks in X80 and X100 Pipe Steels in Near-Neutral pH Environment. Journal of Materials Engineering and Performance. 25:227-240. 2016
- Effect of thermal treatment on the corrosion resistance of Type 316L stainless steel exposed in supercritical water. Journal of Nuclear Materials. 464:356-364. 2015
- Effect of ultrasonic impact peening on the corrosion of ferritic–martensitic steels in supercritical water. Journal of Nuclear Materials. 457:266-272. 2015
- Microstructure stability of candidate stainless steels for Gen-IV SCWR fuel cladding application. Journal of Nuclear Materials. 454:7-11. 2014
- Stability of MgO-, CeO2- and SiO2-doped Cr2O3 ceramics in high-temperature supercritical water. Corrosion Science. 82:339-346. 2014
- Effect of surface modification on the corrosion resistance of austenitic stainless steel 316L in supercritical water conditions. Journal of Supercritical Fluids. 81:157-163. 2013
- Effect of yttria addition on the stability of porous chromium oxide ceramics in supercritical water. Journal of Nuclear Materials. 432:466-474. 2013
- Laser and electron beam welding of 25 mm thick a516 gr.70 steel. ICALEO 2013 - 32nd International Congress on Applications of Lasers and Electro-Optics. 351-355. 2013
- Corrosion behavior of chromium oxide based ceramics in supercritical water (SCW) environments. Corrosion Science. 65:461-471. 2012
- Technical Note:Examination of Focused Ion Beam-Sectioned Surface Films Formed on AM60B Mg Alloy in an Aqueous Saline Solution. Corrosion. 68:468-474. 2012
- Effect of Some Microstructural Parameters on the Corrosion Resistance of Magnesium Alloys. Magnesium Technology. 271-276. 2012
- Corrosion behavior of porous chromium carbide in supercritical water. Journal of Nuclear Materials. 420:320-327. 2012
- Deposition, characterization and performance evaluation of ceramic coatings on metallic substrates for supercritical water-cooled reactors. Surface and Coatings Technology. 205:3512-3519. 2011
- Corrosion and ion release behavior of ultra-fine grained bulk pure copper fabricated by ECAP in Hanks solution as potential biomaterial for contraception. Materials Letters. 64:524-527. 2010
- Stress corrosion cracking of oil and gas pipelines in near neutral pH environment: review of recent research. Energy Materials: Materials Science and Engineering for Energy Systems. 3:220-226. 2008
- Corrosion protection of magnesium alloys by cold spray. Advanced Materials and Processes. 165:53-54. 2007
- Low-alloy steels for reinforcing rods in concrete. MATERIALS PERFORMANCE. 46:56-61. 2007
- Carbon‐Nanotube‐Based Glucose/O2 Biofuel Cells. Advanced Materials. 18:2639-2643. 2006
- Corrosion-resistant rockbolts for underground structures. MATERIALS PERFORMANCE. 40:60-64. 2001
- Temperature dependence of magnetic properties of SmCo/FeCo multilayer films. Journal of Materials Science and Technology. 16:199-200. 2000
- Surface cracking and phase transformations associated with cathodic charging of austenitic stainless steel. Materials Science and Technology. 10:817-822. 1994
- The effect of hydrogen on the fracture of a commercial duplex stainless steel. Corrosion Science. 32:23-36. 1991
- Stress Corrosion Cracking of Annealed Type 316 Stainless Steel in High-Temperature Water. Corrosion. 46:621-627. 1990
- The stress corrosion cracking behaviour of annealed 316 stainless steel in low oxygen 5 ppm chloride content water at 300°C. Corrosion Science. 30:555-567. 1990
- Synergistic Roles of Nb and Mo in the Formation of Oxides on Fe-20Cr-25Ni-Nb Stainless Steels in High-Temperature CO2. Metals. 13:665-665.
- The Improvement of Surface Properties for Laser Cladding Inconel 625 Coating with Laser Shock Peening. Journal of Materials Engineering and Performance. 1-12.