- The effect of surface grinding and Si addition on the corrosion of Fe-12Cr ODS steels in supercritical CO2. 224:111533-111533. 2023
- Understanding the excellent corrosion resistance of Fe-12Cr ODS alloys with and without Si in supercritical CO2 through advanced characterization. 210:110827-110827. 2023
- Influence of stoichiometry on the corrosion response of titanium oxide coatings produced by plasma electrolytic oxidation. 203:110361-110361. 2022
- Effects of Si, Mn on the corrosion behavior of ferritic–martensitic steels in supercritical water (SCW) environments. 166:108432-108432. 2020
- Silicon effects on the wet oxidation of type 310 stainless steel. 143:376-389. 2018
- Stress corrosion cracking susceptibility of thermally-aged Type 310S stainless steels in supercritical water. 135:1-11. 2018
- Characterization of initial intergranular oxidation processes in alloy 600 at a sub-nanometer scale. 133:36-47. 2018
- A comparative study of oxide scales grown on stainless steel and nickel-based superalloys in ultra-high temperature supercritical water at 800 °C. 106:188-207. 2016
- High resolution analysis of oxidation in Ni-Fe-Cr alloys after exposure to 315 °C deaerated water with added hydrogen. 106:236-248. 2016
- The influence of the high Fe and Cr contents of Alloy 800 on its inter- and intragranular oxidation tendency in 480 °C hydrogenated steam. 106:117-126. 2016
- The reproducibility of corrosion testing in supercritical water—Results of an international interlaboratory comparison exercise. 106:147-156. 2016
- Corrosion of engineering materials in a supercritical water cooled reactor: Characterization of oxide scales on Alloy 800H and stainless steel 316. 100:222-230. 2015
- Oxidation behavior of GTD111 Ni-based superalloy at 900 °C in air. 100:267-274. 2015
- Internal oxidation of Alloy 600 exposed to hydrogenated steam and the beneficial effects of thermal treatment. 86:108-122. 2014
- Role of copper and aluminum on the corrosion behavior of austenitic Fe–Mn–C TWIP steels in aqueous solutions and the related hydrogen absorption. 83:234-244. 2014
- The cathodic behaviour of Al–Mn precipitates during atmospheric and saline aqueous corrosion of a sand-cast AM50 alloy. 83:299-309. 2014
- Role of copper and aluminum additions on the hydrogen embrittlement susceptibility of austenitic Fe–Mn–C TWIP steels. 82:218-226. 2014
- Stability of MgO-, CeO2- and SiO2-doped Cr2O3 ceramics in high-temperature supercritical water. 82:339-346. 2014
- The role of aluminum distribution on the local corrosion resistance of the microstructure in a sand-cast AM50 alloy. 77:151-163. 2013
- Tracking the corrosion of magnesium sand cast AM50 alloy in chloride environments. 75:114-122. 2013
- Corrosion behavior of chromium oxide based ceramics in supercritical water (SCW) environments. 65:461-471. 2012
- Analysis of the surface film formed on Mg by exposure to water using a FIB cross-section and STEM–EDS. 59:222-228. 2012
- Corrosion potential oscillations of nickel-containing stainless steel in concentrated sulphuric acid: II Mechanism and kinetic modelling. 52:250-254. 2010
- Effect of curing characterization on the corrosion performance of polyester and polyester/epoxy powder coatings. 50:3280-3286. 2008
- Corrosion potential oscillation of stainless steel in concentrated sulphuric acid: I. Electrochemical aspects. 48:1560-1570. 2006
- Corrosion of nickel-containing stainless steel in concentrated sulphuric acid. 46:1969-1979. 2004
- Anodic behaviour of stainless steel S43000 in concentrated solutions of sulphuric acid. 45:1571-1594. 2003
- The effect of hydrogen on the fracture of a commercial duplex stainless steel. 32:23-36. 1991
- The stress corrosion cracking behaviour of annealed 316 stainless steel in low oxygen 5 ppm chloride content water at 300°C. 30:555-567. 1990
- De-alloying at elevated temperatures and at 298 k-similarities and differences. 22:621-635. 1982