Abstract

The possibility of surrogating high-pressure supercritical water (SCW) with an ambient pressure air-10% H2O (wet air) mixture for studying wet oxidation of Type 310S stainless steel (UNS S31008) at high temperatures was examined using gravimetric measurements coupled with electron microscopy techniques. A distinctly different wet oxidation kinetic rate law was observed in the two environments at 550°C: parabolic for the wet air mixture and …