publication venue for
- Corrosion behavior of alloy 316L stainless steel after exposure to supercritical water at 500 °C for 20,000 h. 127:191-199. 2017
- Internal oxidation and crack susceptibility of alloy 310S stainless steel after long term exposure to supercritical water at 500°C. 120:161-172. 2017
- A comparative study on the oxidation of austenitic alloys 304 and 304-oxide dispersion strengthened steel in supercritical water at 650 °C. 119:245-260. 2017
- Effect of surface modification on the corrosion resistance of austenitic stainless steel 316L in supercritical water conditions. 81:157-163. 2013