Increasing wet adhesion between cellulose surfaces with polyvinylamine
Abstract
The conditions are elucidated whereby strong adhesive joints between two wet cellulose surfaces can be achieved with a polyelectrolyte adhesive. Adhesion results were obtained with wet, TEMPO oxidized, regenerated cellulose membranes that were laminated with polyvinylamine (PVAm) adhesive. Wet adhesion was determined as the 90° wet-peel delamination force. Aldehyde groups on the oxidized cellulose form imine and aminal covalent linkages with …
Authors
Yang D; Stimpson TC; Soucy J; Esser A; Pelton RH
Journal
Cellulose, Vol. 26, No. 1, pp. 341–353
Publisher
Springer Nature
Publication Date
1 2019
DOI
10.1007/s10570-018-2165-9
ISSN
0969-0239